Materials / Compare

Aluminum 6063-T6 vs. Silicon

Compare Aluminum 6063-T6 vs. Silicon strength, stiffness, weight and thermal properties.

Aluminum 6063-T6Wrought
SiliconGrown single crystal
MechanicalAluminum 6063-T6Silicon
Yield strength215MPa1none (brittle)
Ultimate tensile strength240MPa1modulus of rupture130MPa2
Flexural strengthnot sourcedmodulus of rupture130MPa2
Elongation at break12%1none (brittle)
Young's modulus (stiffness)69GPa1131GPa21.9x stiffer
Density2,700kg/m³12,329kg/m³216% lighter
Strength to weight79.6kN·m/kg43% higher55.8kN·m/kg
Stiffness to weight25.6MN·m/kg56.2MN·m/kg2.2x higher
Poisson's rationot sourced0.2212
Shear modulusnot sourced53.6GPa
Bulk modulusnot sourced78.3GPa
Speed of sound5,055m/s7,500m/s48% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4Ceramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6063-T6Silicon
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4Ceramic Alumina 96%Aluminum A380Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6063-T6Silicon
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 6063-T6Silicon
Thermal conductivity201W/m·K123% more heat through a fin163W/m·K2
Thermal expansion23.4µm/m·K12.62µm/m·K28.93x less
100 mm part over a 50 °C swing117µm growth13.1µm growth8.93x less
Specific heat901J/kg·K323% higher732J/kg·K2
Heats up and cools (diffusivity)82.6mm²/s95.6mm²/s16% faster
Thermal shock resistancenot sourced48,095W/m
Melting pointmelting range615–655°C11,412°C2
Max service temperaturenot sourced300°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4Ceramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6063-T6Silicon
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4Ceramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6063-T6Silicon
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Kaiser Aluminum, Korth Kristalle, Hydro
Aluminum 6063-T6
6063-T6 extruded tube, Kaiser Aluminum Tube & Pipe Alloy 6063 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-6063 extruded-products datasheet (Rev.4, 03/2023).
Silicon
Synthetic single-crystal silicon (cubic, diamond structure), Korth Kristalle (crystal grower) material data; Korth usually supplies Floating Zone (FZ) material, Czochralski (Cz) also offered. Silicon is elastically anisotropic; the producer quotes one modulus and the solver is isotropic.
  1. 1
    Alloy 6063 Tube & Pipe Technical Data, Rev. 05/06Kaiser Aluminumarchived copyAluminum 6063-T6 · Yield strength: typical, T6, 0.0625 in specimenAluminum 6063-T6 · Ultimate tensile strength: typical, T6Aluminum 6063-T6 · Elongation at break: typical, T6, in 4DAluminum 6063-T6 · Young's modulus (stiffness): typicalAluminum 6063-T6 · Density: nominal, 20 °CAluminum 6063-T6 · Thermal conductivity: typical, T6, 20 °CAluminum 6063-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 6063-T6 · Melting point: melting range
  2. 2
    Si: SiliconKorth Kristallearchived copySilicon · Ultimate tensile strength: modulus of rupture (bending fracture stress); brittle, no yield pointSilicon · Flexural strength: modulus of ruptureSilicon · Young's modulus (stiffness): typical (single quoted value of an anisotropic crystal)Silicon · Density: typicalSilicon · Poisson's ratio: typicalSilicon · Thermal conductivity: typical at 313 K (40 °C)Silicon · Thermal expansion: typical at 300 KSilicon · Specific heat: typicalSilicon · Melting point: typicalSilicon · Max service temperature: producer's maximum application temperature (optical components)
  3. 3
    Technical Datasheet, Extruded Products: Alloy EN AW-6063 (Rev. 4, 2023)Hydroarchived copyAluminum 6063-T6 · Specific heat: typical, 20 °C (Hydro EN AW-6063)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 6063-T6 stronger than Silicon?

Aluminum 6063-T6 is stronger: its yield strength is 215 MPa against tensile strength 130 MPa for Silicon (1.65x).

Which is lighter, Aluminum 6063-T6 or Silicon?

Silicon is lighter: 2,329 kg/m³ against 2,700 kg/m³ for Aluminum 6063-T6.

Which is stiffer, Aluminum 6063-T6 or Silicon?

Silicon is stiffer: Young's modulus 131 GPa against 69 GPa for Aluminum 6063-T6, so the same part in Silicon deflects less under the same load.

Which is lighter for the same job, Aluminum 6063-T6 or Silicon?

For the same stiffness or strength: Aluminum 6063-T6 is lighter for a strong rod or tie, strong beam, strong panel or plate; Silicon is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beAluminum 6063-T6Silicon
Stiff rod or tie (tension)2.2x heavierlighter
Stiff beam (bending)1.6x heavierlighter
Stiff panel or plate44% heavierlighter
Strong rod or tielighter43% heavier
Strong beamlighter21% heavier
Strong panel or platelighter11% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Aluminum 6063-T6 or Silicon?

Aluminum 6063-T6 conducts heat better: 201 W/m·K against 163 W/m·K for Silicon.

Which expands less with temperature?

Silicon expands less: 2.62 µm/m·K against 23.4 µm/m·K for Aluminum 6063-T6.