Materials / Plastic

Plastic PBT GF30

Plastic PBT GF30 (Ultradur B 4300 G6) strength, stiffness, density and thermal properties, with their source.

A bracket in Plastic PBT GF30, smooth finish.

Mechanical
Yield strengthnot given (tensile used)
Ultimate tensile strengthstress at break140MPa1
Flexural strength210MPa1
Elongation at breakstrain at break3%1
Young's modulus (stiffness)9.8GPa1
Density1,530kg/m³1
Strength to weight91.5kN·m/kg
Stiffness to weight6.41MN·m/kg
Poisson's rationot sourced
Shear modulusnot sourced
Bulk modulusnot sourced
Speed of sound2,531m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Plastic PBT GF30
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Plastic PBT GF30
Strength against densityHigher and further left: stronger for its weight
Thermal
Thermal conductivity0.27W/m·K1
Thermal expansionlongitudinal25µm/m·K1
100 mm part over a 50 °C swing125µm growth
Specific heat1,050J/kg·K1
Heats up and cools (diffusivity)0.168mm²/s
Thermal shock resistancenot sourced
Melting pointDSC223°C1
Max service temperatureHDT 1.8 MPa205°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Plastic PBT GF30
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PPS GF40Plastic LCP GF30Plastic PBT GF30
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Sources1 document: BASF
Values for
Bulk polymer (molded or machined). BASF Ultradur B 4300 G6 (PBT, 30% glass fibre), injection moulding grade; product information sheet 09/2026, typical values for uncoloured product at 23 °C.
  1. 1
    Ultradur B 4300 G6 Product InformationBASFUltimate tensile strength: stress at break, 23 °CFlexural strength: typical, 23 °CElongation at break: strain at break, 23 °CYoung's modulus (stiffness): typical, 23 °CDensity: typicalThermal conductivity: typical (DIN 52612-1)Thermal expansion: longitudinal (flow), mean 23-55 °CSpecific heat: typical, 23 °CMelting point: DSC (ISO 11357)Max service temperature: HDT 1.8 MPa

Thermal properties of Plastic PBT GF30

Thermal conductivity of Plastic PBT GF30

Plastic PBT GF30 has a thermal conductivity of 0.27 W/m·K (0.156 BTU/hr·ft·°F). Basis: typical (DIN 52612-1). Source: BASF, Ultradur B 4300 G6 Product Information.

Specific heat of Plastic PBT GF30

The specific heat capacity of Plastic PBT GF30 is 1,050 J/kg·K (0.251 BTU/lb·°F). Basis: typical, 23 °C. Source: BASF, Ultradur B 4300 G6 Product Information.

Coefficient of thermal expansion of Plastic PBT GF30

Plastic PBT GF30 expands 25 µm/m·K (13.9 µin/in·°F): a 100 mm part grows 125 µm over a 50 °C rise. Basis: longitudinal (flow), mean 23-55 °C. Source: BASF, Ultradur B 4300 G6 Product Information.

Thermal diffusivity of Plastic PBT GF30

Computed from the conductivity, density and specific heat (k / ρc): 0.168 mm²/s, how fast a temperature change spreads through it.

Melting point of Plastic PBT GF30

Plastic PBT GF30 melts at 223 °C (433 °F). Basis: DSC (ISO 11357). Source: BASF, Ultradur B 4300 G6 Product Information.

Maximum service temperature of Plastic PBT GF30

The maximum service temperature of Plastic PBT GF30 is 205 °C (401 °F). Basis: HDT 1.8 MPa. Source: BASF, Ultradur B 4300 G6 Product Information.