Materials / Compare

Plastic Nylon PA6 vs. Plastic TPU

Compare Plastic Nylon PA6 vs. Plastic TPU strength, stiffness, weight and thermal properties.

Plastic Nylon PA6Bulk polymer (molded or machined)
Plastic TPU3D printed (FDM)
MechanicalPlastic Nylon PA6Plastic TPU
Yield strength90MPa1not given (tensile used)
Ultimate tensile strengthnot stated (yield given)23.7MPa2
Flexural strengthnot sourced4.1MPa2
Elongation at break10%1not sourced
Young's modulus (stiffness)3.5GPa152.2x stiffer0.067GPa2
Density1,130kg/m³11,220kg/m³2
Strength to weight79.6kN·m/kg4.1x higher19.4kN·m/kg
Stiffness to weight3.1MN·m/kg56.4x higher0.0549MN·m/kg
Poisson's ratiobase material0.43not sourced
Shear modulus1.25GPanot sourced
Bulk modulus5.83GPanot sourced
Speed of sound1,760m/s7.51x faster234m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA6Plastic TPU
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA6Plastic TPU
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic Nylon PA6Plastic TPU
Thermal conductivity0.33W/m·K1not sourced
Thermal expansionlongitudinal102µm/m·K1not sourced
100 mm part over a 50 °C swing510µm growthnot sourced
Specific heat1,700J/kg·K1not sourced
Heats up and cools (diffusivity)0.172mm²/snot sourced
Thermal shock resistance49.9W/mnot sourced
Melting pointDSC220°C1217°C2
Max service temperature87°C1HDT 0.455 MPa50.3°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA6
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic Nylon PA6
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: BASF, UltiMaker, Covestro
Plastic Nylon PA6
BASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
Plastic TPU
Ultimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.
  1. 1
    Ultramid B3S Product InformationBASFPlastic Nylon PA6 · Yield strength: typical, dryPlastic Nylon PA6 · Elongation at break: nominal strain at break, dryPlastic Nylon PA6 · Young's modulus (stiffness): typical, dryPlastic Nylon PA6 · Density: typicalPlastic Nylon PA6 · Thermal conductivity: typicalPlastic Nylon PA6 · Thermal expansion: longitudinal, 23-55 °CPlastic Nylon PA6 · Specific heat: typicalPlastic Nylon PA6 · Melting point: DSCPlastic Nylon PA6 · Max service temperature: IEC 60216 temperature index, 20000 h
  2. 2
    Ultimaker TPU 95A Technical Data Sheet, v5.00UltiMakerarchived copyPlastic TPU · Ultimate tensile strength: typical, stress at breakPlastic TPU · Flexural strength: typicalPlastic TPU · Young's modulus (stiffness): typicalPlastic TPU · Density: typicalPlastic TPU · Melting point: typicalPlastic TPU · Max service temperature: HDT 0.455 MPa (printed specimens)
  3. 3
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA6 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic TPU is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Plastic Nylon PA6 stronger than Plastic TPU?

Plastic Nylon PA6 is stronger: its yield strength is 90 MPa against tensile strength 23.7 MPa for Plastic TPU (3.8x).

Which is lighter, Plastic Nylon PA6 or Plastic TPU?

Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 1,220 kg/m³ for Plastic TPU.

Which is stiffer, Plastic Nylon PA6 or Plastic TPU?

Plastic Nylon PA6 is stiffer: Young's modulus 3.5 GPa against 0.067 GPa for Plastic TPU, so the same part in Plastic Nylon PA6 deflects less under the same load.

Which is lighter for the same job, Plastic Nylon PA6 or Plastic TPU?

For the same stiffness or strength: Plastic Nylon PA6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic Nylon PA6Plastic TPU
Stiff rod or tie (tension)lighter56.4x heavier
Stiff beam (bending)lighter7.8x heavier
Stiff panel or platelighter4.04x heavier
Strong rod or tielighter4.1x heavier
Strong beamlighter2.63x heavier
Strong panel or platelighter2.1x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Related comparisons