Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
3
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA6 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Nylon PA6 stronger than Plastic PMMA?
Plastic Nylon PA6 is stronger: its yield strength is 90 MPa against tensile strength 80 MPa for Plastic PMMA (13%).
Which is lighter, Plastic Nylon PA6 or Plastic PMMA?
Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 1,190 kg/m³ for Plastic PMMA.
Which is stiffer, Plastic Nylon PA6 or Plastic PMMA?
Plastic Nylon PA6 is stiffer: Young's modulus 3.5 GPa against 3.3 GPa for Plastic PMMA, so the same part in Plastic Nylon PA6 deflects less under the same load.
Which is lighter for the same job, Plastic Nylon PA6 or Plastic PMMA?
For the same stiffness or strength: Plastic Nylon PA6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic Nylon PA6
Plastic PMMA
Stiff rod or tie (tension)
lighter
12% heavier
Stiff beam (bending)
lighter
8% heavier
Stiff panel or plate
lighter
7% heavier
Strong rod or tie
lighter
18% heavier
Strong beam
lighter
14% heavier
Strong panel or plate
lighter
12% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic Nylon PA6 or Plastic PMMA?
Plastic Nylon PA6 stretches further before it breaks: 10% elongation at break against 5.5% for Plastic PMMA.
Thermal
Which conducts heat better, Plastic Nylon PA6 or Plastic PMMA?
Plastic Nylon PA6 conducts heat better: 0.33 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature?
Plastic PMMA expands less: 70 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.