Plastic PMMA vs. Plastic PPS GF40 Compare Plastic PMMA vs. Plastic PPS GF40 strength, stiffness, weight and thermal properties.
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Plastic PMMA Bulk polymer (molded or machined) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Plastic PPS GF40 Bulk polymer (molded or machined) Mechanical Plastic PMMA Plastic PPS GF40 Yield strength not given (tensile used) not given (tensile used) Ultimate tensile strength 80 MPa tensile strength 195 MPa 2.44x stronger Compressive strength 110 MPa not sourced Flexural strength 115 MPa 285 MPa Elongation at break 5.5 % 2.89x more ductile strain at break 1.9 % Young's modulus (stiffness) 3.3 GPa 14.7 GPa 4.45x stiffer Density 1,190 kg/m³ 39% lighter 1,650 kg/m³ Strength to weight 67.2 kN·m/kg 118 kN·m/kg 1.76x higher Stiffness to weight 2.77 MN·m/kg 8.91 MN·m/kg 3.21x higher Poisson's ratio 0.37 0.35 Shear modulus 1.2 GPa 5.44 GPa 4.52x stiffer in shear Bulk modulus 4.23 GPa 16.3 GPa 3.86x higher Speed of sound 1,665 m/s 2,985 m/s 1.79x faster
1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic LCP GF30 Plastic PMMA Plastic PPS GF40 Stiffness against densityHigher and further left: stiffer for its weight 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic LCP GF30 Plastic PMMA Plastic PPS GF40 Strength against densityHigher and further left: stronger for its weight
Thermal Plastic PMMA Plastic PPS GF40 Thermal conductivity 0.19 W/m·K 0.2 W/m·K Thermal expansion 0-50 °C 70 µm/m·K parallel 12 µm/m·K 5.83x less 100 mm part over a 50 °C swing 350 µm growth 60 µm growth 5.83x less Specific heat 1,470 J/kg·K not sourced Heats up and cools (diffusivity) 0.109 mm²/s not sourced Thermal shock resistance 41.5 W/m 144 W/m 3.47x more resistant Melting point not sourced DSC 280 °C Glass transition not sourced DSC 90 °C Max service temperature 80 °C HDT 1.8 MPa 270 °C
1k 10k 0.1 1 10 100 Density (kg/m³) Thermal conductivity (W/m·K) Plastic PLA Plastic PETG Plastic ABS Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic LCP GF30 Plastic PMMA Plastic PPS GF40 Thermal conductivity against densityHigher and further left: spreads more heat for its weight 0.1 1 10 100 10 100 Thermal conductivity (W/m·K) Thermal expansion (µm/m·K) Plastic PETG Plastic ABS Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic LCP GF30 Plastic PMMA Plastic PPS GF40 Thermal expansion against thermal conductivityLower and further right: warps less when heated
Sources 3 documents: Röhm, Celanese
Plastic PMMA Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
Plastic PPS GF40 Celanese Fortron 1140L4 (PPS, 40% glass fibre), injection moulding; FORTRON PPS Short-Term Properties Guide (PPS-012, 2016); thermal conductivity and Poisson for 40% glass-reinforced Fortron from the Fortron PPS Design Manual (PPS-050, 2013). 1 PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1) Röhm archived copy Plastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature2 Fortron PPS Short-Term Properties Guide (PPS-012) Celanese Plastic PPS GF40 · Ultimate tensile strength: tensile strength, 5 mm/minPlastic PPS GF40 · Flexural strength: flexural strength at breakPlastic PPS GF40 · Elongation at break: strain at break, 5 mm/minPlastic PPS GF40 · Young's modulus (stiffness): typical, 1 mm/minPlastic PPS GF40 · Density: typicalPlastic PPS GF40 · Thermal expansion: parallel (flow), mean -50 to 90 °CPlastic PPS GF40 · Melting point: DSC, 10 °C/minPlastic PPS GF40 · Glass transition: DSC, 10 °C/minPlastic PPS GF40 · Max service temperature: HDT 1.8 MPa
3 Fortron PPS Design Manual (PPS-050) Celanese Plastic PPS GF40 · Poisson's ratio: glass-reinforced Fortron PPS (class value, not grade-specific)Plastic PPS GF40 · Thermal conductivity: 40% glass-reinforced Fortron, 25 °C (not grade-specific)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions Mechanical Is Plastic PMMA stronger than Plastic PPS GF40? Plastic PPS GF40 is stronger: its tensile strength is 195 MPa against 80 MPa for Plastic PMMA (2.44x).
Which is lighter, Plastic PMMA or Plastic PPS GF40? Plastic PMMA is lighter: 1,190 kg/m³ against 1,650 kg/m³ for Plastic PPS GF40.
Which is stiffer, Plastic PMMA or Plastic PPS GF40? Plastic PPS GF40 is stiffer: Young's modulus 14.7 GPa against 3.3 GPa for Plastic PMMA, so the same part in Plastic PPS GF40 deflects less under the same load.
Which is lighter for the same job, Plastic PMMA or Plastic PPS GF40? For the same stiffness or strength: Plastic PPS GF40 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be Plastic PMMA Plastic PPS GF40 Stiff rod or tie (tension) 3.21x heavier lighter Stiff beam (bending) 1.52x heavier lighter Stiff panel or plate 19% heavier lighter Strong rod or tie 1.76x heavier lighter Strong beam 31% heavier lighter Strong panel or plate 13% heavier lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PMMA or Plastic PPS GF40? Plastic PMMA stretches further before it breaks: 5.5% elongation at break against 1.9% for Plastic PPS GF40.
Thermal Which conducts heat better, Plastic PMMA or Plastic PPS GF40? Plastic PPS GF40 conducts heat better: 0.2 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature? Plastic PPS GF40 expands less: 12 µm/m·K against 70 µm/m·K for Plastic PMMA.