Materials / Compare

Plastic PETG vs. Plastic PPS GF40

Compare Plastic PETG vs. Plastic PPS GF40 strength, stiffness, weight and thermal properties.

Plastic PETG3D printed (FDM)
Plastic PPS GF40Bulk polymer (molded or machined)
MechanicalPlastic PETGPlastic PPS GF40
Yield strength46.2MPa1not given (tensile used)
Ultimate tensile strength46.2MPa1tensile strength195MPa24.22x stronger
Flexural strength78.9MPa1285MPa2
Elongation at break7.6%14x more ductilestrain at break1.9%2
Young's modulus (stiffness)1.94GPa114.7GPa27.58x stiffer
Density1,270kg/m³130% lighter1,650kg/m³2
Strength to weight36.4kN·m/kg118kN·m/kg3.25x higher
Stiffness to weight1.53MN·m/kg8.91MN·m/kg5.84x higher
Poisson's rationot sourced0.353
Shear modulusnot sourced5.44GPa
Bulk modulusnot sourced16.3GPa
Speed of sound1,236m/s2,985m/s2.42x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PETGPlastic PPS GF40
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PETGPlastic PPS GF40
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic PETGPlastic PPS GF40
Thermal conductivitybase material0.21W/m·K40.2W/m·K3
Thermal expansionbase material51µm/m·K4parallel12µm/m·K24.25x less
100 mm part over a 50 °C swing255µm growth60µm growth4.25x less
Specific heatbase material1,300J/kg·K4not sourced
Heats up and cools (diffusivity)0.127mm²/snot sourced
Thermal shock resistancenot sourced144W/m
Melting pointnot sourcedDSC280°C2
Glass transition77.4°C1DSC90°C212.6 °C higher
Max service temperatureHDT 0.455 MPa76.2°C1HDT 1.8 MPa270°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PETGPlastic PPS GF40
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PETGPlastic PPS GF40
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: UltiMaker, Celanese, Eastman
Plastic PETG
Ultimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.
Plastic PPS GF40
Celanese Fortron 1140L4 (PPS, 40% glass fibre), injection moulding; FORTRON PPS Short-Term Properties Guide (PPS-012, 2016); thermal conductivity and Poisson for 40% glass-reinforced Fortron from the Fortron PPS Design Manual (PPS-050, 2013).
  1. 1
    Ultimaker PETG Technical Data Sheet, v1.00UltiMakerarchived copyPlastic PETG · Yield strength: typicalPlastic PETG · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic PETG · Flexural strength: typicalPlastic PETG · Elongation at break: typicalPlastic PETG · Young's modulus (stiffness): typicalPlastic PETG · Density: typicalPlastic PETG · Glass transition: typicalPlastic PETG · Max service temperature: HDT 0.455 MPa (printed specimens)
  2. 2
    Fortron PPS Short-Term Properties Guide (PPS-012)CelanesePlastic PPS GF40 · Ultimate tensile strength: tensile strength, 5 mm/minPlastic PPS GF40 · Flexural strength: flexural strength at breakPlastic PPS GF40 · Elongation at break: strain at break, 5 mm/minPlastic PPS GF40 · Young's modulus (stiffness): typical, 1 mm/minPlastic PPS GF40 · Density: typicalPlastic PPS GF40 · Thermal expansion: parallel (flow), mean -50 to 90 °CPlastic PPS GF40 · Melting point: DSC, 10 °C/minPlastic PPS GF40 · Glass transition: DSC, 10 °C/minPlastic PPS GF40 · Max service temperature: HDT 1.8 MPa
  3. 3
    Fortron PPS Design Manual (PPS-050)CelanesePlastic PPS GF40 · Poisson's ratio: glass-reinforced Fortron PPS (class value, not grade-specific)Plastic PPS GF40 · Thermal conductivity: 40% glass-reinforced Fortron, 25 °C (not grade-specific)
  4. 4
    Eastar Copolyester 6763 Product Data SheetEastmanPlastic PETG · Thermal conductivity: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Thermal expansion: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Specific heat: base material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Plastic PETG stronger than Plastic PPS GF40?

Plastic PPS GF40 is stronger: its tensile strength is 195 MPa against yield strength 46.2 MPa for Plastic PETG (4.22x).

Which is lighter, Plastic PETG or Plastic PPS GF40?

Plastic PETG is lighter: 1,270 kg/m³ against 1,650 kg/m³ for Plastic PPS GF40.

Which is stiffer, Plastic PETG or Plastic PPS GF40?

Plastic PPS GF40 is stiffer: Young's modulus 14.7 GPa against 1.94 GPa for Plastic PETG, so the same part in Plastic PPS GF40 deflects less under the same load.

Which is lighter for the same job, Plastic PETG or Plastic PPS GF40?

For the same stiffness or strength: Plastic PPS GF40 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PETGPlastic PPS GF40
Stiff rod or tie (tension)5.84x heavierlighter
Stiff beam (bending)2.12x heavierlighter
Stiff panel or plate1.51x heavierlighter
Strong rod or tie3.25x heavierlighter
Strong beam2.01x heavierlighter
Strong panel or plate1.58x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PETG or Plastic PPS GF40?

Plastic PETG stretches further before it breaks: 7.6% elongation at break against 1.9% for Plastic PPS GF40.

Thermal

Which conducts heat better, Plastic PETG or Plastic PPS GF40?

Plastic PETG conducts heat better: 0.21 W/m·K against 0.2 W/m·K for Plastic PPS GF40.

Which expands less with temperature?

Plastic PPS GF40 expands less: 12 µm/m·K against 51 µm/m·K for Plastic PETG.

Related comparisons