Materials / Compare

Ceramic Alumina 96% vs. Steel A992

Compare Ceramic Alumina 96% vs. Steel A992 strength, stiffness, weight and thermal properties.

Ceramic Alumina 96%Sintered ceramic (pressed and fired)
Steel A992Wrought
MechanicalCeramic Alumina 96%Steel A992
Yield strengthnone (brittle)385MPa1
Ultimate tensile strength221MPa2505MPa12.29x stronger
Compressive strength2,068MPa2not sourced
Flexural strengthflexural strength358MPa2not sourced
Elongation at breaknone (brittle)24.2%1
Young's modulus (stiffness)303GPa2design value200GPa3
Density3,720kg/m³22.11x lighter7,850kg/m³4
Strength to weight59.4kN·m/kg21% higher49kN·m/kg
Stiffness to weight81.5MN·m/kg3.2x higher25.5MN·m/kg
Poisson's ratio0.212design value0.33
Shear modulus125GPa1.63x stiffer in shear76.9GPa
Bulk modulus174GPa4% higher167GPa
Speed of sound9,025m/s1.79x faster5,048m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Steel A992
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Steel A992
Strength against densityHigher and further left: stronger for its weight
ThermalCeramic Alumina 96%Steel A992
Thermal conductivity24.7W/m·K248W/m·K41.94x more heat through a fin
Thermal expansionmean8.2µm/m·K246% less12µm/m·K4
100 mm part over a 50 °C swing41µm growth46% less60µm growth
Specific heat880J/kg·K2base material460–480J/kg·K5
Heats up and cools (diffusivity)7.55mm²/s13mm²/s1.72x faster
Thermal shock resistance1,736W/m5,390W/m3.11x more resistant
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Steel A992
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Steel A992
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: American Institute of Steel Construction, CoorsTek, bauforumstahl (ArcelorMittal), Ovako
Ceramic Alumina 96%
CoorsTek AD-96, nominal 96% Al2O3 sintered alumina, typical values; CoorsTek "Ceramic Seal Material Properties" (© 2018, 01899 F). AD-96 is the general 96% grade, not the ADS-96R substrate grade.
Steel A992
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
  1. 1
    Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
  2. 2
    Ceramic Seal Material Properties (01899 F)CoorsTekarchived copyCeramic Alumina 96% · Ultimate tensile strength: typical tensile strength, 25 °C (ACMA Test #4)Ceramic Alumina 96% · Compressive strength: typical, 20 °C (ASTM-C773)Ceramic Alumina 96% · Flexural strength: flexural strength (MOR), 20 °C (ASTM-F417)Ceramic Alumina 96% · Young's modulus (stiffness): typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Density: typical (ASTM-C20)Ceramic Alumina 96% · Poisson's ratio: typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Thermal conductivity: typical, 20 °C (ASTM-C408)Ceramic Alumina 96% · Thermal expansion: mean, 25-1000 °C (ASTM-C372)Ceramic Alumina 96% · Specific heat: typical, 100 °C (ASTM-E1269)
  3. 3
    ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
  4. 4
    Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
  5. 5
    S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Ceramic Alumina 96% stronger than Steel A992?

Steel A992 is stronger: its yield strength is 385 MPa against tensile strength 221 MPa for Ceramic Alumina 96% (1.74x).

Which is lighter, Ceramic Alumina 96% or Steel A992?

Ceramic Alumina 96% is lighter: 3,720 kg/m³ against 7,850 kg/m³ for Steel A992.

Which is stiffer, Ceramic Alumina 96% or Steel A992?

Ceramic Alumina 96% is stiffer: Young's modulus 303 GPa against 200 GPa for Steel A992, so the same part in Ceramic Alumina 96% deflects less under the same load.

Which is lighter for the same job, Ceramic Alumina 96% or Steel A992?

For the same stiffness or strength: Ceramic Alumina 96% is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCeramic Alumina 96%Steel A992
Stiff rod or tie (tension)lighter3.2x heavier
Stiff beam (bending)lighter2.6x heavier
Stiff panel or platelighter2.42x heavier
Strong rod or tielighter21% heavier
Strong beamlighter46% heavier
Strong panel or platelighter1.6x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Ceramic Alumina 96% or Steel A992?

Steel A992 conducts heat better: 48 W/m·K against 24.7 W/m·K for Ceramic Alumina 96%.

Which expands less with temperature?

Ceramic Alumina 96% expands less: 8.2 µm/m·K against 12 µm/m·K for Steel A992.

Related comparisons