Materials / Compare

Aluminum 1100-O vs. Copper C10100

Compare Aluminum 1100-O vs. Copper C10100 strength, stiffness, weight and thermal properties.

Aluminum 1100-OWrought
Copper C10100Wrought
MechanicalAluminum 1100-OCopper C10100
Yield strength35MPa169MPa21.97x stronger
Ultimate tensile strength90MPa1221MPa22.46x stronger
Elongation at break35%145%229% more ductile
Young's modulus (stiffness)69GPa1117GPa21.7x stiffer
Density2,710kg/m³13.3x lighter8,941kg/m³2
Strength to weight12.9kN·m/kg1.67x higher7.72kN·m/kg
Stiffness to weight25.5MN·m/kg1.94x higher13.1MN·m/kg
Poisson's rationot sourced0.343
Shear modulusnot sourced43.7GPa
Bulk modulusnot sourced122GPa
Speed of sound5,046m/s39% faster3,621m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OCopper C10100
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OCopper C10100
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 1100-OCopper C10100
Thermal conductivity222W/m·K1391W/m·K21.76x more heat through a fin
Thermal expansion23.6µm/m·K116.9µm/m·K240% less
100 mm part over a 50 °C swing118µm growth84.5µm growth40% less
Specific heatbase material901J/kg·K42.34x higher385J/kg·K2
Heats up and cools (diffusivity)90.9mm²/s114mm²/s25% faster
Thermal shock resistancenot sourced8,992W/m
Melting pointmelting range640–655°C1melting point1,083°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OCopper C10100
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OCopper C10100
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Kaiser Aluminum, Copper Development Association, Wieland, Hydro
Aluminum 1100-O
1100-O (annealed) commercially pure aluminium, Kaiser Aluminum Tube & Pipe Alloy 1100 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-1050A (99.5% Al) extruded-products datasheet (10/2018).
Copper C10100
C10100 oxygen-free electronic (OFE) copper, annealed to 0.050 mm grain size (OS050), 0.04 in. flat products, copper.org typical values
  1. 1
    Alloy 1100 Tube & Pipe Technical Data, Rev. 05/06Kaiser Aluminumarchived copyAluminum 1100-O · Yield strength: typical, O, 0.0625 in specimenAluminum 1100-O · Ultimate tensile strength: typical, OAluminum 1100-O · Elongation at break: typical, O, in 4DAluminum 1100-O · Young's modulus (stiffness): typicalAluminum 1100-O · Density: nominal, 20 °CAluminum 1100-O · Thermal conductivity: typical, O, 20 °CAluminum 1100-O · Thermal expansion: typical, mean 20-100 °CAluminum 1100-O · Melting point: melting range
  2. 2
    C10100 Alloy (copper.org)Copper Development Associationarchived copyCopper C10100 · Yield strength: typical, 0.5% extension under load, 0.04 in. flatCopper C10100 · Ultimate tensile strength: typical, 0.04 in. flatCopper C10100 · Elongation at break: typical, 0.04 in. flatCopper C10100 · Young's modulus (stiffness): typicalCopper C10100 · Density: nominalCopper C10100 · Thermal conductivity: typical, 20 °CCopper C10100 · Thermal expansion: typical, mean 20-100 °CCopper C10100 · Specific heat: typical, 20 °CCopper C10100 · Melting point: melting point (liquidus = solidus, pure copper)
  3. 3
    Wieland-K09 (Cu-OFE, C10100) Data SheetWielandCopper C10100 · Poisson's ratio: reference value at room temperature (Wieland-K09 = Cu-OFE = C10100, rolled products)
  4. 4
    Technical Datasheet, Extruded Products: Alloy EN AW-1050AHydroAluminum 1100-O · Specific heat: base material: commercially pure aluminium EN AW-1050A (Hydro), 20 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 1100-O stronger than Copper C10100?

Copper C10100 is stronger: its yield strength is 69 MPa against 35 MPa for Aluminum 1100-O (1.97x).

Which is lighter, Aluminum 1100-O or Copper C10100?

Aluminum 1100-O is lighter: 2,710 kg/m³ against 8,941 kg/m³ for Copper C10100.

Which is stiffer, Aluminum 1100-O or Copper C10100?

Copper C10100 is stiffer: Young's modulus 117 GPa against 69 GPa for Aluminum 1100-O, so the same part in Copper C10100 deflects less under the same load.

Which is lighter for the same job, Aluminum 1100-O or Copper C10100?

For the same stiffness or strength: Aluminum 1100-O is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 1100-OCopper C10100
Stiff rod or tie (tension)lighter1.94x heavier
Stiff beam (bending)lighter2.53x heavier
Stiff panel or platelighter2.77x heavier
Strong rod or tielighter1.67x heavier
Strong beamlighter2.1x heavier
Strong panel or platelighter2.35x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 1100-O or Copper C10100?

Copper C10100 stretches further before it breaks: 45% elongation at break against 35% for Aluminum 1100-O.

Thermal

Which conducts heat better, Aluminum 1100-O or Copper C10100?

Copper C10100 conducts heat better: 391 W/m·K against 222 W/m·K for Aluminum 1100-O.

Which expands less with temperature?

Copper C10100 expands less: 16.9 µm/m·K against 23.6 µm/m·K for Aluminum 1100-O.