A bracket in Plastic ABS (bulk/injection), smooth finish.
| Mechanical | |
|---|---|
| Yield strength | 45MPa1 |
| Flexural strength | 65MPa1 |
| Elongation at break | 10%1 |
| Young's modulus (stiffness) | 2.3GPa1 |
| Density | 1,040kg/m³1 |
| Strength to weight | 43.3kN·m/kg |
| Stiffness to weight | 2.21MN·m/kg |
| Poisson's ratio | 0.392 |
| Shear modulus | 0.827GPa |
| Bulk modulus | 3.48GPa |
| Speed of sound | 1,487m/s |
| Thermal | |
|---|---|
| Thermal conductivity | 0.17W/m·K1 |
| Thermal expansion | range80–110µm/m·K1 |
| 100 mm part over a 50 °C swing | 475µm growth |
| Specific heat | not sourced |
| Heats up and cools (diffusivity) | not sourced |
| Thermal shock resistance | 21.4W/m |
| Max service temperature | HDT 1.8 MPa94°C1 |
Sources2 documents: INEOS Styrolution, Covestro
- Values for
- Bulk polymer (molded or machined). INEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)
- 1Terluran GP-22 (ABS) Product Data SheetINEOS StyrolutionYield strength: typical, tensile stress at yield 23 °CFlexural strength: typical, 23 °CElongation at break: nominal strain at break, 23 °CYoung's modulus (stiffness): typicalDensity: typicalThermal conductivity: typicalThermal expansion: rangeMax service temperature: HDT 1.8 MPa (annealed 4 h/80 °C)
- 2Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPoisson's ratio: typical, ABS family (Covestro Part and Mold Design guide, Table 3-1)
Thermal properties of Plastic ABS (bulk/injection)
Thermal conductivity of Plastic ABS (bulk/injection)
Plastic ABS (bulk/injection) has a thermal conductivity of 0.17 W/m·K (0.0982 BTU/hr·ft·°F). Basis: typical. Source: INEOS Styrolution, Terluran GP-22 (ABS) Product Data Sheet.
Coefficient of thermal expansion of Plastic ABS (bulk/injection)
Plastic ABS (bulk/injection) expands 80–110 µm/m·K (44.4–61.1 µin/in·°F): a 100 mm part grows 475 µm over a 50 °C rise. Basis: range. Source: INEOS Styrolution, Terluran GP-22 (ABS) Product Data Sheet.
Maximum service temperature of Plastic ABS (bulk/injection)
The maximum service temperature of Plastic ABS (bulk/injection) is 94 °C (201 °F). Basis: HDT 1.8 MPa (annealed 4 h/80 °C). Source: INEOS Styrolution, Terluran GP-22 (ABS) Product Data Sheet.
Compare Plastic ABS (bulk/injection) with
Other Plastic
- Plastic ABS (bulk/injection) vs. Plastic PLA
- Plastic ABS (bulk/injection) vs. Plastic PETG
- Plastic ABS (bulk/injection) vs. Plastic ABS
- Plastic ABS (bulk/injection) vs. Plastic TPU
- Plastic ABS (bulk/injection) vs. Plastic Nylon
- Plastic ABS (bulk/injection) vs. Plastic Polycarbonate
- Plastic ABS (bulk/injection) vs. Plastic POM/Acetal
- Plastic ABS (bulk/injection) vs. Plastic Nylon PA6
- Plastic ABS (bulk/injection) vs. Plastic Nylon PA66
- Plastic ABS (bulk/injection) vs. Plastic PEEK
- Plastic ABS (bulk/injection) vs. Plastic PTFE
- Plastic ABS (bulk/injection) vs. Plastic UHMWPE
- Plastic ABS (bulk/injection) vs. Plastic HDPE
- Plastic ABS (bulk/injection) vs. Plastic Polypropylene
- Plastic ABS (bulk/injection) vs. Plastic PMMA
- Plastic ABS (bulk/injection) vs. Plastic PBT GF30
- Plastic ABS (bulk/injection) vs. Plastic PPS GF40
- Plastic ABS (bulk/injection) vs. Plastic LCP GF30
Closest alternatives
- Plastic ABS (bulk/injection) vs. FDM ASA
- Plastic ABS (bulk/injection) vs. FDM Polycarbonate
- Plastic ABS (bulk/injection) vs. SLA Resin Tough 2000
- Plastic ABS (bulk/injection) vs. SLS PA12 Nylon
- Plastic ABS (bulk/injection) vs. SLA Resin Standard
- Plastic ABS (bulk/injection) vs. Rubber
- Plastic ABS (bulk/injection) vs. FDM PAHT-CF
- Plastic ABS (bulk/injection) vs. FDM HIPS